Strength Of Material Lab

Creep Testing Machine

Creep Testing Machine

Model No – MI-SML-0060

Table unit for the investigation of the creep behavior of different materials Flat specimens made of lead and PP Specimen cross-section 2 Ã- 5 mm, measured length 25 mm
Tensile stress range 5…25N/mm2
Position measurement gauge 0…10mm
Resolution 0.01mm
Experiments above or below room temperature possible with conditioning box
Specimen
Material: lead, PP
Cross-section: 2 Ã- 5 mm
Measured length: 25mm
Tensile stress range: 5.25N/mm2
Position measurement
-Range: 0…10mm
-Resolution 0.01 mm